PA66 40-45% Mineral Filled Material Data Sheet

PA66 40-45% Mineral Filled (Polyamide 66) Material Data Sheet

PA66 40-45% Mineral Filled Overview

PA66 40-45% mineral filled is a grade of polyamide 66 (PA66, nylon 66), designated Polyamide (Nylon) (Type 66, 40-45% Mineral Filled). This PA66 40-45% mineral filled material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.

PA66 40-45% Mineral Filled Designation

Polyamide (Nylon) (Type 66, 40-45% Mineral Filled)
TradenamesAdell, Akulon, Altech, Ashlene, Bergamid, Chemlon, Denyl, Minlon, Nilamid, Nycal, Nymax, Nypol, Plustek, Radilon, Scanamid, Slovamid, Staramide, Ultramid, Wellamid

PA66 40-45% Mineral Filled Typical uses

Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.

PA66 40-45% Mineral Filled Composition detail

Polymer55–60%
Mineral (unspecified)40–45%

PA66 40-45% Mineral Filled Physical properties

Density1.48–1.51g/cm3

PA66 40-45% Mineral Filled Mechanical properties

Young’s modulus3.61–4.51GPa
Specific stiffness2.41–3.02MN.m/kg
Yield strength (elastic limit)49.8–62.2MPa
Tensile strength50.4–61.6MPa
Specific strength33.3–41.6kN.m/kg
Elongation8.62–12.4% strain
Elongation at yield6.89–13.1% strain
Compressive modulus3.86–4.26GPa
Compressive strength63.8–70.6MPa
Flexural modulus3.69–4.42GPa
Flexural strength (modulus of rupture)69.9–85.5MPa
Shear modulus1.44–1.51GPa
Shear strength30.2–37MPa
Bulk modulus5.27–5.83GPa
Poisson’s ratio0.363–0.378 
Shape factor6.62
Hardness – Vickers16–18HV
Hardness – Rockwell M107–118 
Hardness – Rockwell R107–118 
Hardness – Shore D79–82 
Elastic stored energy (springs)304–485kJ/m3
Fatigue strength at 10^7 cycles21.3–23.5MPa

PA66 40-45% Mineral Filled Impact & fracture properties

Fracture toughness4.06–4.49MPa.m0.5
Toughness (G)3.91–5.23kJ/m2
Impact strength, notched 23 °C5.61–10.9kJ/m2
Impact strength, notched -30 °C3.46–7.52kJ/m2
Impact strength, unnotched 23 °C208–305kJ/m2
Impact strength, unnotched -30 °C164–246kJ/m2

PA66 40-45% Mineral Filled Thermal properties

Melting point250–265°C
Glass temperature54–66°C
Heat deflection temperature 0.45MPa160–249°C
Heat deflection temperature 1.8MPa149–226°C
Maximum service temperature90–130°C
Minimum service temperature-81–-71°C
Thermal conductivity0.386–0.418W/m.°C
Specific heat capacity1350–1400J/kg.°C
Thermal expansion coefficient47.7–49.5µstrain/°C
Thermal shock resistance243–331°C
Thermal distortion resistance0.00791–0.00864MW/m

PA66 40-45% Mineral Filled Electrical properties

Electrical resistivity2.87e19–7.18e20µohm.cm
Electrical conductivity2.4e-19–6.01e-18%IACS
Dielectric constant (relative permittivity)7.76–10.9 
Dissipation factor (dielectric loss tangent)0.127–0.334 
Dielectric strength (dielectric breakdown)31.8–54.2MV/m
Comparative tracking index500–600V

PA66 40-45% Mineral Filled Magnetic properties

Magnetic typeNon-magnetic

PA66 40-45% Mineral Filled Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity1550–1740m/s
Mechanical loss coefficient (tan delta)0.0125–0.0138 

PA66 40-45% Mineral Filled Absorption & permeability

Water absorption @ 24 hrs0.45–0.74%
Water absorption @ sat3.9–5.2%
Humidity absorption @ sat1.2–1.6%

PA66 40-45% Mineral Filled Processing properties

Polymer injection moldingExcellent
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage1.2 – 2.2 %
Melt temperature223 – 304 °C
Mold temperature70 – 100 °C
Molding pressure range34.4 – 138 MPa

PA66 40-45% Mineral Filled Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisAcceptable
Organic solventsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Poor
FlammabilitySlow-burning