Home » PEKK (Polyetherketoneketone) » PEKK 40% Glass Fiber Material Data Sheet
PEKK 40% Glass Fiber (Polyetherketoneketone) Material Data Sheet
PEKK 40% Glass Fiber Overview
PEKK 40% glass fiber is a grade of polyetherketoneketone (PEKK), designated Polyetherketoneketone (40% glass fiber). This PEKK 40% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEKK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEKK parts in-house and inspects them before shipment.
PEKK Designation
Polyetherketoneketone (40% glass fiber) Tradenames Oxpekk
PEKK 40% Glass Fiber Composition detail
Polymer 60 % Glass (fiber) 40 %
PEKK Physical properties
PEKK 40% Glass Fiber Mechanical properties
Young’s modulus 12.5 – 21.3 GPa Specific stiffness 7.77 – 13.2 MN.m/kg Yield strength (elastic limit) 152 – 163 MPa Tensile strength 188 – 202 MPa Specific strength 94.4 – 101 kN.m/kg Elongation 1.54 – 1.96 % strain Elongation at yield 1.5 – 2 % strain Compressive modulus 12.5 – 21.3 GPa Flexural modulus 12 – 14.9 GPa Flexural strength (modulus of rupture) 273 – 293 MPa Shear modulus 4.6 – 7.9 GPa Shear strength 85 – 94 MPa Poisson’s ratio 0.41 – 0.45 Shape factor 8.4 Hardness – Vickers 45 – 48 HV Elastic stored energy (springs) 578 – 996 kJ/m3 Fatigue strength at 10^7 cycles 74.1 – 81.9 MPa
PEKK Impact & fracture properties
Impact strength, notched 23 °C 9.63 – 11.8 kJ/m2 Impact strength, unnotched 23 °C 81.6 – 99.8 kJ/m2
PEKK 40% Glass Fiber Thermal properties
Melting point 347 – 373 °C Glass temperature 154 – 172 °C Heat deflection temperature 0.45MPa 322 – 336 °C Heat deflection temperature 1.8MPa 314 – 328 °C Vicat softening point 322 – 336 °C Maximum service temperature 233 – 287 °C Specific heat capacity 1230 – 1250 J/kg.°C Thermal expansion coefficient 10.7 – 11.3 µstrain/°C Thermal shock resistance 671 – 1150 °C
PEKK Electrical properties
Electrical resistivity 9250000000000000 – 10800000000000000 µohm.cm Electrical conductivity 1.6e-14 – 1.86e-14 %IACS Dielectric constant (relative permittivity) 3.17 – 3.43 Dissipation factor (dielectric loss tangent) 0.0035 – 0.0045 Dielectric strength (dielectric breakdown) 23 – 25 MV/m
PEKK Magnetic properties
Magnetic type Non-magnetic
PEKK Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2760 – 3670 m/s
PEKK Absorption & permeability
Water absorption @ 24 hrs 0.072 – 0.088 %
PEKK Processing properties
Polymer injection molding Acceptable Polymer extrusion Limited use Polymer thermoforming Unsuitable Linear mold shrinkage 0.15 – 0.25 % Melt temperature 376 – 383 °C Mold temperature 132 – 249 °C Molding pressure range 103 – 138 MPa
PEKK Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Unacceptable Weak alkalis Excellent Strong alkalis Excellent Organic solvents Excellent Oils and fuels Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Excellent Flammability Self-extinguishing
Modulus Metal Services
Manufacturing & Quality Services in Turkey