PEKK Unfilled Amorphous (Polyetherketoneketone) Material Data Sheet
PEKK Unfilled Amorphous Overview
PEKK unfilled amorphous is a grade of polyetherketoneketone (PEKK), designated Polyetherketoneketone (unfilled, amorphous). This PEKK unfilled amorphous material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEKK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEKK parts in-house and inspects them before shipment.
PEKK Designation
Polyetherketoneketone (unfilled, amorphous) Tradenames Oxpekk, Pyramid
PEKK Unfilled Amorphous Composition detail
PEKK Physical properties
PEKK Unfilled Amorphous Mechanical properties
Young’s modulus 3.36 – 3.53 GPa Specific stiffness 2.62 – 2.77 MN.m/kg Yield strength (elastic limit) 98 – 108 MPa Tensile strength 85.1 – 94.1 MPa Specific strength 76.5 – 84.5 kN.m/kg Elongation 74 – 86 % strain Elongation at yield 5 – 7 % strain Compressive modulus 3.36 – 3.53 GPa Compressive strength 97.8 – 108 MPa Flexural modulus 3.29 – 3.46 GPa Flexural strength (modulus of rupture) 135 – 141 MPa Shear modulus 1.2 – 1.3 GPa Shear strength 98 – 108 MPa Poisson’s ratio 0.39 – 0.43 Shape factor 4.3 Hardness – Vickers 25 – 28 HV Elastic stored energy (springs) 1390 – 1690 kJ/m3 Fatigue strength at 10^7 cycles 34 – 37.6 MPa
PEKK Impact & fracture properties
Impact strength, notched 23 °C 4.32 – 5.28 kJ/m2 Impact strength, unnotched 23 °C 35 – 42 kJ/m2
PEKK Unfilled Amorphous Thermal properties
Glass temperature 146 – 163 °C Heat deflection temperature 0.45MPa 136 – 153 °C Heat deflection temperature 1.8MPa 133 – 149 °C Vicat softening point 136 – 153 °C Maximum service temperature 233 – 287 °C Thermal conductivity 0.25 W/m.°C Specific heat capacity 1550 – 1580 J/kg.°C Thermal expansion coefficient 75.1 – 78.9 µstrain/°C Thermal shock resistance 365 – 412 °C Thermal distortion resistance 0.00317 – 0.00333 MW/m
PEKK Electrical properties
Electrical resistivity 9250000000000000 – 10800000000000000 µohm.cm Electrical conductivity 1.6e-14 – 1.86e-14 %IACS Dielectric constant (relative permittivity) 3.17 – 3.43 Dissipation factor (dielectric loss tangent) 0.0035 – 0.0045 Dielectric strength (dielectric breakdown) 23 – 25 MV/m
PEKK Magnetic properties
Magnetic type Non-magnetic
PEKK Optical, aesthetic and acoustic properties
Transparency Transparent Acoustic velocity 1620 – 1660 m/s
PEKK Absorption & permeability
Water absorption @ 24 hrs 0.18 – 0.22 %
PEKK Processing properties
Polymer injection molding Acceptable Polymer extrusion Limited use Polymer thermoforming Unsuitable Linear mold shrinkage 0.4 – 0.6 %
PEKK Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Unacceptable Weak alkalis Excellent Strong alkalis Excellent Organic solvents Excellent Oils and fuels Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Excellent Flammability Self-extinguishing