C14200 Tough-Pitch Arsenical H.C. Copper, Soft Material Data Sheet
C14200 Tough-Pitch Arsenical H.C. Copper Material Data Sheet (Wrought, Soft)
C14200 Soft Tough-Pitch Arsenical Overview
C14200 soft tough-pitch arsenical is a wrought general purpose copper (UNS C14200, EN CW117C, C107), known as tough-pitch arsenical h.c. copper. Condition: Soft. This C14200 soft tough-pitch arsenical material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for C14200 copper parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined C14200 copper parts in-house and inspects them before shipment.
Stress corrosion cracking Note: Rated in ammoniacal; Other susceptible environments: Water, amine, dinitrogen tetroxide
Not susceptible
C14200 Notes
C14200 Soft Tough-Pitch Arsenical Other notes
(s)=soft; (1/2 h)=half hard; (h)=hard; (xh)=extra hard; (hr) = hot rolled; (w)=soln heat-trtd; (wh)=soln heat-trtd & work hdnd; (wp)=soln heat-trtd & precip hdnd; (whp)=precip hdnd after cold-wkng; (wph)=work hdnd after precip hdng.
C14200 Standards with similar compositions
International: CuAs(P) to ISO 1635, CuAs(P) to ISO 1637, CuAs(P) to ISO 1640
Switzerland: Cu-DPA to VSM 11557/1
USA: C14200, C14200 to ASTM B111M, C14200 to ASTM B152M, C14200 to ASTM B359M, C14200 to ASTM B379, C14200 to ASTM B395M, C14200 to ASTM B447, C14200 to ASTM B75M, UNS C14100, UNS C14200, UNS C14210