ADI 1050 Austempered Ductile Cast Iron Mechanical Properties

ADI 1050 Mechanical properties

Young’s modulus160–168GPa
Specific stiffness22.6–23.7MN.m/kg
Yield strength (elastic limit)730–866MPa
Tensile strength1050–1200MPa
Specific strength103–122kN.m/kg
Elongation6–10% strain
Compressive modulus160–168GPa
Compressive strength1530–1790MPa
Flexural modulus160–168GPa
Flexural strength (modulus of rupture)835–954MPa
Shear modulus59.4–69.1GPa
Shear strength950–1.11e3MPa
Bulk modulus105–110GPa
Poisson’s ratio0.24–0.25 
Shape factor2.03   
Hardness – Vickers320–363HV
Hardness – Brinell320–363HB
Elastic stored energy (springs)1630–2280kJ/m^3
Fatigue strength at 10^7 cycles398–469MPa

ADI 1050 Impact & fracture properties

Fracture toughness77–93MPa.m^0.5
Toughness (G)36.4–52.4kJ/m^2

Designation: ADI 1050 Austempered Ductile Cast Iron

ADI 1050
Condition                                                                                              Cast and austempered

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey