ADI 1050 Austempered Ductile Cast Iron Equivalent Grades

ADI 1050 Equivalent Grades Standards with similar compositions EN 1564 EN-GJS-1050-6 ASTM A897 1050-750-07 ISO17804/JS/1050-6 Designation: ADI 1050 Austempered Ductile Cast Iron ADI 1050 Condition                                                                                              Cast and austempered MODULUS METALSand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection … Continue reading ADI 1050 Austempered Ductile Cast Iron Equivalent Grades