ADI 1050 Austempered Ductile Cast Iron Thermal Properties

ADI 1050 Thermal Properties Melting point 1110 – 1190 °C Maximum service temperature 350 – 450 °C Minimum service temperature 0     °C Thermal conductivity 21 – 22.6 W/m.°C Specific heat capacity 460 – 495 J/kg.°C Thermal expansion coefficient 12.3 – 16.3 µstrain/°C Thermal shock resistance 291 – 403 °C Thermal distortion resistance 1.33 … Continue reading ADI 1050 Austempered Ductile Cast Iron Thermal Properties