Bronze CuMn13Al9 Chemical Composition (cast, aluminum bronze)

Designation: CuMn13Al9

Typical uses: Heavy and intricate items with high resistance to corrosion and wear, used at raised temperatures.

Composition detail : Bronze CuMn13Al9 Chemical Composition (cast, aluminum bronze)

Al (aluminum)8.5–9.5%
Cu (copper)66.9–77%
Fe (iron)2–4%
Mn (manganese)11–14%
Ni (nickel)1.5–4.5%
Pb (lead)0–0.02%
Si (silicon)0–0.1%
Sn (tin)0–1%
Typical uses: Bronze CuMn13Al9 Chemical Composition (cast, aluminum bronze)
Heavy and intricate items with high resistance to corrosion and wear, used at raised temperatures.

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey