Bronze CuMn13Al9 Mechanical Properties (cast, aluminum bronze)

Designation: CuMn13Al9 Mechanical properties: Bronze CuMn13Al9 Mechanical Properties (cast, aluminum bronze) Young’s modulus 119 – 122 GPa Specific stiffness 15.6 – 16.6 MN.m/kg Yield strength (elastic limit) 380 – 470 MPa Tensile strength 740 – 820 MPa Specific strength 50.5 – 62.9 kN.m/kg Elongation 9 – 20 % strain Compressive strength 380 – 470 MPa … Continue reading Bronze CuMn13Al9 Mechanical Properties (cast, aluminum bronze)