Bronze CuAl10Fe3 Chemical Composition (C95200, cast aluminum bronze)

Designation
CuAl10Fe3
UNS numberC95200
EN nameCC331G
ISO nameCuAl10FE3
GB (Chinese) nameCuAl10Fe3
JIS (Japanese) nameAl BC 1

Bronze CuAl10Fe3 Chemical Composition (C95200, cast aluminum bronze)

Al (aluminum)8.5–9.5%
Cu (copper)86.5–89%
Fe (iron)2.5–4%


MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey