| Fracture Toughness & Toughness | Values |
|---|---|
| Fracture toughness | *133 – 147 MPa.m^0.5 |
| Toughness (G) | *89.9 – 110 kJ/m^2 |
| *Values indicated with asterisks (*) are approximate. No guarantee is provided for the precision of this information. | |