AISI 204-Cu Stainless steel, Annealed, Austenitic | Mechanical Properties
Modulus Metal | Manufacturer Company in TURKEY: Sand Casting | Investment Casting | Foundry | CNC Machining | Press Bending | Laser Cutting | Welding | Plastics Injection Molding |Turkiye Mechanical properties Values Young’s modulus * 193 – 201 GPa Specific stiffness * 24.7 – 25.7 MN.m/kg Yield strength (elastic limit) 324 – 415 MPa Tensile … Continue reading AISI 204-Cu Stainless steel, Annealed, Austenitic | Mechanical Properties