| Composition detail | % |
|---|---|
| C (carbon) | 0 – 0.03 % |
| Cr (chromium) | 16 – 18 % |
| Fe (iron) | * 67.9 – 75 % |
| Mn (manganese) | 5.5 – 7.5 % |
| N (nitrogen) | 0 – 0.25 % |
| Ni (nickel) | 3.5 – 5.5 % |
| P (phosphorus) | 0 – 0.045 % |
| S (sulfur) | 0 – 0.03 % |
| Si (silicon) | 0 – 0.75 % |