Low Carbon steel, AISI 1015 annealed (Plain Carbon, 0.15%C) Equivalent Grades | Sand Casting | Investment Casting | Foundry | CNC Machining | Supplier Company | Modulus Metal in TURKEY

Carbon steel, AISI 1015, annealed Equivalent Grades,Sand Casting,Investment Casting,Machining, Turkey,Modulus Metal

Low Carbon Steel General Info

The most affordable of all structural metals is low-carbon steel, usually referred to as mild steel. It is utilized extensively for a variety of purposes.

Strengths
Very low cost, superior to higher carbon steels in terms of toughness, machinability, formability, and weldability. Cold-working improves machinability and strength.

Limitations
Low strength and poor hardenability as compared to higher carbon steels.

Designation
The AISI/SAE designations for carbon steels are 10xx, 11xx, 12xx, and 15xx. Low carbon steels have carbon contents as indicated by the last two numbers, which can reach 30. The EN designations 1.03zz and 1.04zz apply to low carbon steels.

Common uses
Numerous applications, including the reinforcement of concrete, building sections, roofing sheets, vehicle body panels, and cans.

Low Carbon steel, AISI 1015 annealed Equivalent Grades
UNS numberG10150
US nameASTM MT1015, ASTM M1015, ASTM G10170, ASTM 1015, ASME G10150, ~SAE SAE J525, ~SAE SAE J524, ~SAE SAE J356, ~ASTM A822, ~ASTM A214, ~ASTM A2
EN nameHS17, ~UkSt37-2, ~P235T1, ~C15R, ~C15E, ~C15
EN number~1.1141, ~1.1140, ~1.0124
ISO name~R33, ~CE15E4, ~CC15X, ~CC15A
GB (Chinese) name~ML15Al, ~CRB650
JIS (Japanese) nameSWRM 17, SWRM 15, SWRCH17R, SWRCH15R, SGD 3, ~SWRCH15A

© Modulus Metal 2017-2022    |    All Rights Reserved