Young’s modulus 165 – 178 GPa
Flexural modulus * 165 – 178 GPa
Shear modulus 64 – 71 GPa
Bulk modulus 119 – 135 GPa
Poisson’s ratio 0.27 – 0.28
Shape factor 23
Yield strength (elastic limit) 320 – 370 MPa
Tensile strength 500 – 600 MPa
Compressive strength * 351 – 382 MPa
Flexural strength (modulus of rupture) 339 – 372 MPa
Elongation 7 – 15 % strain
Hardness – Vickers 175 – 225 HV
Fatigue strength at 10^7 cycles 224 – 248 MPa
Fatigue strength model (stress range) 142 – 190 MPa
Parameters: Stress Ratio = 0, Number of Cycles = 1e7
Fracture toughness * 22 – 54 MPa.m^0.5
Mechanical loss coefficient (tan delta) * 0.001 – 0.0014