Cast iron, nodular graphite, EN GJS 500 7 Equivalent Grades | Modulus Metal | Supplier | Foundry | Castings Products | in TURKEY

NBN 830-02 FNG42-12 (Belgium)GB 1348(88) QT 400-15 (China)GB 1348(88) QT 450-10 (China)IS 1865 SG400/12 (India)UNI 4544 GS400-12 (Italy)JIS G5502(95) FCD40 Class 1 (Japan)AS 1831(85) 400-12 (NSW Australia)SABS 936 SG42 (South Africa)BS 2789 420/12 (United Kingdom)ASTM A536(93) 65-45-12 (USA)SAE J434 D4512 (USA)