EN GJL 150 Cast iron, gray, flake graphite, Mechanical Properties
Young’s modulus 90 – 109 GPa
Flexural modulus * 90 – 109 GPa
Shear modulus 35 – 44 GPa
Bulk modulus 61 – 78 GPa
Poisson’s ratio 0.255 – 0.265
Shape factor 25
Yield strength (elastic limit) 97 – 117 MPa
Tensile strength 150 – 250 MPa
Compressive strength * 190 – 235 MPa
Flexural strength (modulus of rupture) * 110 – 140 MPa
Elongation 0.45 – 0.6 % strain
Hardness – Vickers 105 – 265 HV
Fatigue strength at 10^7 cycles 40 – 80 MPa
Fatigue strength model (stress range) 27.6 – 66.6 MPa
Parameters: Stress Ratio = 0, Number of Cycles = 1e7
Fracture toughness * 19 – 23 MPa.m^0.5
Mechanical loss coefficient (tan delta) 0.01 – 0.035
*Values are approximations. This information’s accuracy is not guaranteed.