Young’s modulus 165 – 173 GPa
Flexural modulus * 165 – 173 GPa
Shear modulus 64 – 69 GPa
Bulk modulus 119 – 132 GPa
Poisson’s ratio 0.27 – 0.28
Shape factor 24
Yield strength (elastic limit) 250 – 305 MPa
Tensile strength 400 – 450 MPa
Compressive strength * 292 – 319 MPa
Flexural strength (modulus of rupture) 278 – 305 MPa
Elongation 12 – 20 % strain
Hardness – Vickers 145 – 165 HV
Fatigue strength at 10^7 cycles 201 – 210 MPa
Fatigue strength model (stress range) 126 – 152 MPa
Parameters: Stress Ratio = 0, Number of Cycles = 1e7
Fracture toughness 33 – 54 MPa.m^0.5
Mechanical loss coefficient (tan delta) * 0.0014 – 0.0018
*Values are approximations. This information’s accuracy is not guaranteed.
Furnace Modulus Metal Sand Casting Investment Casting Foundry Pouring Gray Ductile Nodular Products Parts Manufacturing Machining CNC Supplier in Turkey Turquie

© Modulus Metal 2017-2022    |    All Rights Reserved