Young’s modulus 165 – 173 GPa
Flexural modulus * 165 – 173 GPa
Shear modulus 64 – 69 GPa
Bulk modulus 119 – 132 GPa
Poisson’s ratio 0.27 – 0.28
Shape factor 23
Yield strength (elastic limit) 305 – 339 MPa
Tensile strength 450 – 500 MPa
Compressive strength * 319 – 351 MPa
Flexural strength (modulus of rupture) 305 – 339 MPa
Elongation 10 – 18 % strain
Hardness – Vickers 160 – 180 HV
Fatigue strength at 10^7 cycles 210 – 224 MPa
Fatigue strength model (stress range) 136 – 162 MPa
Parameters: Stress Ratio = 0, Number of Cycles = 1e7
Fracture toughness * 22 – 54 MPa.m^0.5
Mechanical loss coefficient (tan delta) * 0.0012 – 0.0016
*Values are approximations. This information’s accuracy is not guaranteed.