EN GJS 500 7 Cast iron, nodular graphite, Mechanical Properties |
---|
Young’s modulus 165 – 178 GPa |
Flexural modulus * 165 – 178 GPa |
Shear modulus 64 – 71 GPa |
Bulk modulus 119 – 135 GPa |
Poisson’s ratio 0.27 – 0.28 |
Shape factor 23 |
Yield strength (elastic limit) 320 – 370 MPa |
Tensile strength 500 – 600 MPa |
Compressive strength * 351 – 382 MPa |
Flexural strength (modulus of rupture) 339 – 372 MPa |
Elongation 7 – 15 % strain |
Hardness – Vickers 175 – 225 HV |
Fatigue strength at 10^7 cycles 224 – 248 MPa |
Fatigue strength model (stress range) 142 – 190 MPa Parameters: Stress Ratio = 0, Number of Cycles = 1e7 |
Fracture toughness * 22 – 54 MPa.m^0.5 |
Mechanical loss coefficient (tan delta) * 0.001 – 0.0014 |
*Values are approximations. This information’s accuracy is not guaranteed. |