EN GJS 400 15U <30mm Cast iron, nodular graphite, Mechanical Properties |
---|
Young’s modulus 165 – 173 GPa |
Flexural modulus * 165 – 173 GPa |
Shear modulus 64 – 69 GPa |
Bulk modulus 119 – 132 GPa |
Poisson’s ratio 0.27 – 0.28 |
Shape factor 24 |
Yield strength (elastic limit) 250 – 305 MPa |
Tensile strength 400 – 450 MPa |
Compressive strength * 292 – 319 MPa |
Flexural strength (modulus of rupture) 278 – 305 MPa |
Elongation 12 – 20 % strain |
Hardness – Vickers 145 – 165 HV |
Fatigue strength at 10^7 cycles 201 – 210 MPa |
Fatigue strength model (stress range) 126 – 152 MPa Parameters: Stress Ratio = 0, Number of Cycles = 1e7 |
Fracture toughness 33 – 54 MPa.m^0.5 |
Mechanical loss coefficient (tan delta) * 0.0014 – 0.0018 |