PA69 (Polyamide 69 / Nylon 69)

PA69 (Polyamide 69 / Nylon 69)

PA69 Strengths

PA69 (nylon 69) has a lower density and absorbs less water than PA6 or PA66.

PA69 Limitations

It costs slightly more than PA6 or PA66.

PA69 Designation

PA69, also written 6.9 or 6/9.

Typical Uses of PA69

General mechanical parts of the kind made from nylon 6 or nylon 66 that need better dimensional stability.

PA69 Compositional Summary

(NH-(CH2)6-NH-CO-(CH2)7-CO)n
Material familyPlastic (thermoplastic, semi-crystalline)
Base materialPA69 (Polyamide / nylon 69)
CAS number28757-63-3

PA69 Parts from Turkey

Looking for PA69 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA69 parts in-house and inspects them before shipment.

PA69 Grades

PA69 Unfilled Grades

PA69 Unfilled Grade Material Data Sheet