PA410 Molding and Extrusion Material Data Sheet

PA410 Molding and Extrusion (Polyamide 410) Material Data Sheet

PA410 Molding and Extrusion Overview

PA410 molding and extrusion is a grade of polyamide 410 (PA410, nylon 410), designated Polyamide (Nylon) (Type 410). This PA410 molding and extrusion material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA410 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA410 parts in-house and inspects them before shipment.

PA410 Molding and Extrusion Designation

Polyamide (Nylon) (Type 410)
TradenamesEcoPaXX®

PA410 Molding and Extrusion Typical uses

General purpose, automotive parts, engine covers, fuel tanks, tubing, wheels, household goods, sporting goods, electrical components

PA410 Molding and Extrusion Composition detail

Polymer100  %

PA410 Molding and Extrusion Physical properties

Density1.09–1.1g/cm3

PA410 Molding and Extrusion Mechanical properties

Young’s modulus1.6–1.68GPa
Specific stiffness1.46–1.53MN.m/kg
Yield strength (elastic limit)55–64.2MPa
Tensile strength40–46.7MPa
Specific strength50.2–58.6kN.m/kg
Elongation50–72% strain
Elongation at yield15–21.6% strain
Compressive modulus1.6–1.68GPa
Compressive strength55–64.2MPa
Flexural modulus1.4–1.47GPa
Flexural strength (modulus of rupture)55–64.2MPa
Shear modulus1.6–1.68GPa
Shear strength24–28MPa
Bulk modulus1.8–1.84GPa
Poisson’s ratio0.34–0.36 
Shape factor1.94
Hardness – Vickers17–18.7HV
Hardness – Shore D72–78 
Elastic stored energy (springs)926–1250kJ/m3
Fatigue strength at 10^7 cycles16–18.7MPa

PA410 Molding and Extrusion Impact & fracture properties

Fracture toughness3.23–3.91MPa.m0.5
Toughness (G)6.41–9.26kJ/m2
Impact strength, notched 23 °C13–20kJ/m2
Impact strength, notched -30 °C3.5–3.6kJ/m2
Impact strength, unnotched 23 °C590–600kJ/m2
Impact strength, unnotched -30 °C590–600kJ/m2

PA410 Molding and Extrusion Thermal properties

Melting point250  °C
Glass temperature52.3–66.3°C
Heat deflection temperature 0.45MPa165–185°C
Heat deflection temperature 1.8MPa67–87°C
Vicat softening point182–202°C
Maximum service temperature192–210°C
Minimum service temperature-64–-54°C
Thermal conductivity0.231–0.25W/m.°C
Specific heat capacity1430–1480J/kg.°C
Thermal expansion coefficient70–90µstrain/°C
Thermal shock resistance394–529°C
Thermal distortion resistance0.00266–0.00345MW/m

PA410 Molding and Extrusion Electrical properties

Electrical resistivity1e20  µohm.cm
Electrical conductivity1.72e-18 %IACS
Dielectric constant (relative permittivity)5.16–5.59 
Dissipation factor (dielectric loss tangent)0.208–0.3 
Dielectric strength (dielectric breakdown)28.6–31.5MV/m
Comparative tracking index571–630V

PA410 Molding and Extrusion Magnetic properties

Magnetic typeNon-magnetic

PA410 Molding and Extrusion Optical, aesthetic and acoustic properties

TransparencyTransparent
Acoustic velocity1210–1240m/s
Mechanical loss coefficient (tan delta)0.018–0.0238 

PA410 Molding and Extrusion Absorption & permeability

Water absorption @ 24 hrs0.505–0.611%
Water absorption @ sat5.27–6.38%
Humidity absorption @ sat1.9–2%
Water vapor transmission0.958–1.73g.mm/m².day
Permeability (O2)0.622–1.15cm³.mm/m².day.atm

PA410 Molding and Extrusion Processing properties

First commercial production2010
Polymer injection moldingExcellent
Polymer extrusionAcceptable
Polymer thermoformingLimited use
Linear mold shrinkage1.2 – 1.3 %
Melt temperature270 – 300 °C
Mold temperature60 – 100 °C

PA410 Molding and Extrusion Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsAcceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisLimited use
Organic solventsExcellent
Oils and fuelsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySlow-burning

PA410 Molding and Extrusion Notes

PA410 Molding and Extrusion Other notes
Polyamide 410 is 70% derived from castor oil. It has excellent mechanical properties, high heat stability and outstanding chemical resistance. Polyamide 410 also offers low permeability to both oxygen and water vapor; and and low moisture absorption for improved dimensional stability post conditioning. The impact modified grades offer improved impact resistance making them suitable for sports and leisure applications.