PA410 Impact Modified Grade Material Data Sheet

PA410 Impact Modified Grade (Polyamide 410) Material Data Sheet

PA410 Impact Modified Grade Overview

PA410 impact modified grade is a grade of polyamide 410 (PA410, nylon 410), designated Polyamide (Nylon) (Type 410, impact modified). This PA410 impact modified grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA410 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA410 parts in-house and inspects them before shipment.

PA410 Impact Modified Grade Designation

Polyamide (Nylon) (Type 410, impact modified)
TradenamesEcoPaXX®

PA410 Impact Modified Grade Typical uses

General purpose, automotive parts, engine covers, fuel tanks, tubing, wheels, household goods, sporting goods, electrical components

PA410 Impact Modified Grade Composition detail

Polymer85–95%
Impact modifier5–15%

PA410 Impact Modified Grade Physical properties

Density1.04–1.06g/cm3

PA410 Impact Modified Grade Mechanical properties

Young’s modulus0.9–0.946GPa
Specific stiffness0.856–0.902MN.m/kg
Yield strength (elastic limit)35–40.8MPa
Tensile strength35–40.8MPa
Specific strength33.3–38.9kN.m/kg
Elongation50–72% strain
Elongation at yield20–28.8% strain
Compressive modulus0.9–0.945GPa
Compressive strength35–40.8MPa
Flexural modulus0.95–0.998GPa
Flexural strength (modulus of rupture)40–46.7MPa
Shear modulus0.9–0.945GPa
Shear strength21–24.5MPa
Bulk modulus1.01–1.03GPa
Poisson’s ratio0.34–0.36 
Shape factor1.94
Hardness – Vickers11–12HV
Hardness – Shore D72–78 
Elastic stored energy (springs)666–899kJ/m3
Fatigue strength at 10^7 cycles14–16.3MPa

PA410 Impact Modified Grade Impact & fracture properties

Fracture toughness2.88–3.48MPa.m0.5
Toughness (G)9.05–13kJ/m2
Impact strength, notched 23 °C62–75kJ/m2
Impact strength, notched -30 °C9–20kJ/m2
Impact strength, unnotched 23 °C590–600kJ/m2
Impact strength, unnotched -30 °C590–600kJ/m2

PA410 Impact Modified Grade Thermal properties

Melting point250  °C
Glass temperature52.3–66.3°C
Heat deflection temperature 0.45MPa140–164°C
Heat deflection temperature 1.8MPa65.5–85.5°C
Vicat softening point157–182°C
Maximum service temperature192–210°C
Minimum service temperature-64–-54°C
Thermal conductivity0.231–0.25W/m.°C
Specific heat capacity1370–1430J/kg.°C
Thermal expansion coefficient120–140µstrain/°C
Thermal shock resistance283–353°C
Thermal distortion resistance0.0017–0.00202MW/m

PA410 Impact Modified Grade Electrical properties

Electrical resistivity9.09e19–1.1e20µohm.cm
Electrical conductivity1.57e-18–1.9e-18%IACS
Dielectric constant (relative permittivity)5.16–5.59 
Dissipation factor (dielectric loss tangent)0.208–0.3 
Dielectric strength (dielectric breakdown)28.6–31.5MV/m
Comparative tracking index571–630V

PA410 Impact Modified Grade Magnetic properties

Magnetic typeNon-magnetic

PA410 Impact Modified Grade Optical, aesthetic and acoustic properties

TransparencyTransparent
Acoustic velocity925–950m/s
Mechanical loss coefficient (tan delta)0.024–0.0317 

PA410 Impact Modified Grade Absorption & permeability

Water absorption @ 24 hrs0.455–0.55%
Water absorption @ sat5.27–6.38%
Humidity absorption @ sat1.55–1.87%
Water vapor transmission0.865–1.46g.mm/m².day
Permeability (O2)0.339–0.995cm³.mm/m².day.atm

PA410 Impact Modified Grade Processing properties

First commercial production2010
Polymer injection moldingExcellent
Polymer extrusionAcceptable
Polymer thermoformingLimited use
Linear mold shrinkage1 – 1.2 %
Melt temperature270 – 300 °C
Mold temperature60 – 100 °C

PA410 Impact Modified Grade Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsAcceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisLimited use
Organic solventsExcellent
Oils and fuelsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySlow-burning

PA410 Impact Modified Grade Notes

PA410 Impact Modified Grade Other notes
Polyamide 410 is 70% derived from castor oil. It has excellent mechanical properties, high heat stability and outstanding chemical resistance. Polyamide 410 also offers low permeability to both oxygen and water vapor; and and low moisture absorption for improved dimensional stability post conditioning.