Iron, commercial purity, ingot iron, annealed, >99.9%Fe

Ingot Iron Annealed Mechanical Properties

Young’s modulus204–212GPa
Specific stiffness25.9–26.9MN.m/kg
Yield strength (elastic limit)110–165MPa
Tensile strength230–295MPa
Specific strength14–21kN.m/kg
Elongation35–55% strain
Compressive strength110–165MPa
Flexural modulus204–212GPa
Flexural strength (modulus of rupture)110–165MPa
Shear modulus78–84GPa
Bulk modulus160–178GPa
Poisson’s ratio0.29–0.3 
Shape factor66   
Hardness – Vickers65–85HV
Hardness – Rockwell B15–20HRB
Elastic stored energy (springs)30.1–63.3kJ/m^3
Fatigue strength at 10^7 cycles90–150MPa
Fatigue strength model (stress range)82.6–163MPa

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey