EN GJN HV600 (XCr23) Equivalent Grades, former BS 3D, Cast iron, white, high-chromium alloy

UNS numberF45009
EN GJN HV600 (XCr23), former BS 3D, Cast iron, white, high-chromium alloy Equivalent Grades

Designation

BS EN 12513:2011 EN GJN HV600 (XCr23) (former BS 3D). Record based on BS 4844:1986 BS grade 3D

Standards with similar compositions:

GB 8491(87) KmTBCr26 (China)
AFNOR NFA32401 FBCr26MoNi (France)
DIN G-X260Cr27 (Germany)
DIN G-X300CrMo271 (Germany)
DIN WNr 0.9650 (Germany)
DIN WNr 0.9655 (Germany)
IS 4771-3 HCr27/400 (India)
IS 4771-3 HCrNi27/400 (India)
SIS 140466 466 (Sweden)
BS 4844 3D (United Kingdom)
BS 4844 3E (United Kingdom)

Typical uses

Abrasion resistant components, typically in mineral-pulverizing mills, e.g. grinding balls, drum liner plates, spiral classifier-shoes, pulverizing-bars.