EN GJN HV600 (XCr23) Chemical Composition, former BS 3D, Cast iron, white, high-chromium alloy

Compositional summary

Fe59-76 / Cr22-28 / C1.8-3.6 / Mn0.15-1.5 (impurities: Mo<3, Cu<2, Ni<2, Si<1, P<0.1, S<0.1)

Material family: Metal (ferrous)

Base material: Fe (Iron)

ElementsMinMax%
C (carbon)1.83.6%
Cr (chromium)2228%
Cu (copper)02%
Fe (iron)58.876.1%
Mn (manganese)0.151.5%
Mo (molybdenum)03%
Ni (nickel)02%
P (phosphorus)00.1%
S (sulfur)00.1%
Si (silicon)01%
EN GJN HV600 (XCr23) Chemical Composition, former BS 3D, Cast iron, white, high-chromium alloy