| UNS number | F45001 |
Designation
BS EN 12513:2011 EN GJN HV520 (former BS 2A). Record based on BS 4844:1986 BS grade 2A.
Standards with similar compositions:
| GB 8491(87) KmTBNi4Cr2-DT (China) |
| AFNOR NFA32401 FBNi4Cr2BC (France) |
| DIN G-X260NiCr42 (Germany) |
| DIN WNr 0.9620 (Germany) |
| IS 4771-1A NiLCr30/500 (India) |
| SIS 140512 512 (Sweden) |
| BS 4844 2A (United Kingdom) |
| ASTM A532/A532M(93a) Ni-Cr-Lc (USA) |
Typical uses
Abrasion resistant components, typically in mineral-pulverizing mills, e.g. grinding balls, drum liner plates, spiral classifier-shoes, pulverizing-bars.