EN GJN HV520 Chemical Composition, former BS 2A, Cast iron, white, Ni-Cr alloy

Compositional summary Fe86-93 / Ni3-5.5 / C2.5-3 / Cr1.5-3.5 (impurities: Mn<0.8, Si<0.8, Mo<0.5, P<0.2, S<0.15) Material family: Metal (ferrous) Base material: Fe (Iron) Elements Min Max % C (carbon) 2.5 3 % Cr (chromium) 1.5 3.5 % Fe (iron) 85.7 93 % Mn (manganese) 0 0.8 % Mo (molybdenum) 0 0.5 % Ni (nickel) 3 … Continue reading EN GJN HV520 Chemical Composition, former BS 2A, Cast iron, white, Ni-Cr alloy