| Designation | CuMn13Al8 |
| UNS number | C95700 |
| ISO name | CuMn13Al8Fe3Ni3 |
| JIS (Japanese) name | AlBz4 |
Composition detail : Bronze CuMn13Al8 Chemical Composition (C95700, Cast Aluminum bronze)
| Al (aluminum) | 7 | – | 8.5 | % |
| Cu (copper) | 70.4 | – | 78.5 | % |
| Fe (iron) | 2 | – | 4 | % |
| Mn (manganese) | 11 | – | 14 | % |
| Ni (nickel) | 1.5 | – | 3 | % |
| Pb (lead) | 0 | – | 0.03 | % |
| Si (silicon) | 0 | – | 0.1 | % |
| Typical uses |
| Heavy and intricate items with high resistance to corrosion and wear, used at raised temperatures. |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey