| Designation | |
| C95800 (Nickel Aluminum Bronze) | |
| Condition | As cast |
| UNS number | C95800 |
| US name | C95800 to ASTM B30, ASTM B505, ASTM B763, ASTM B806, ASTM B148, SAE J462 |
| EN name | 2.0976, GB-CuAl10Ni to DIN 17656; U-A9N5FeY200 to NF A53-709 |
| JIS (Japanese) name | AlBC3, AlBC3C, CAC703 to JIS H5114, JIS H5121; AlBCIn2 to JIS H2206 |
Bronze CuAl10Ni5Fe4Mn1 Equivalent Grades (C95800, cast aluminum bronze)
| C95800 to ASTM B30, ASTM B505, ASTM B763, ASTM B806, ASTM B148, SAE J462 |
| 2.0976, GB-CuAl10Ni to DIN 17656 |
| U-A9N5FeY200 to NF A53-709 |
| AlBC3, AlBC3C, CAC703 to JIS H5114, JIS H5121 |
| AlBCIn2 to JIS H2206 |
| 5716-15 to SIS 145716 |
| CuAl10Ni6Fe4 to SABS 200 |
| 16570 to NS 16570 |
| Ampco 483, MTEK 230-N |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey