| Property | Value Range |
|---|---|
| Young’s Modulus | 68.6 – 71.4 GPa |
| Specific Stiffness | 25.3 – 26.4 MN.m/kg |
| Yield Strength (Elastic Limit) | 204 – 232 MPa |
| Tensile Strength | 247 – 252 MPa |
| Specific Strength | 75.3 – 85.6 kN.m/kg |
| Elongation | 3 – 3.6 % strain |
| Compressive Strength | 204 – 232 MPa |
| Flexural Modulus | 68.6 – 71.4 GPa |
| Flexural Strength (Modulus of Rupture) | 204 – 232 MPa |
| Shear Modulus | 25.6 – 27 GPa |
| Bulk Modulus | 64.2 – 73.5 GPa |
| Poisson’s Ratio | 0.322 – 0.338 |
| Shape Factor | 29 |
| Hardness – Vickers | 92 – 102 HV |
| Elastic Stored Energy (Springs) | 298 – 383 kJ/m³ |
| Fatigue Strength at 10⁷ Cycles | 55.8 – 68.2 MPa |
| Fatigue Strength Model (Stress Range) | 55.7 – 68.3 MPa |