Aluminum 355.0, Sand Cast, T6: General Information
Property | Details |
---|---|
Designation | 355.0 (Aluminum Association) |
Condition | T6 (Solution heat-treated and artificially aged) |
UNS Number | A03550 |
EN Number | EN AC-45300 / EN AC-Al Si5Cu1Mg |
Aluminum 355.0, Sand Cast, T6: General Information UNS A03550 General Information | AlSi5Cu1Mg to ISO 3522 General Information |
Typical Uses of Aluminum 355.0 Sand Cast T6
Application | Details |
---|---|
Engine cooling fans | Used in high-performance engines. |
Clutch housings | Durable under high-stress conditions. |
High-speed rotating parts | Suitable for aerospace and industrial. |
Structural aerospace components | Lightweight and strong for aviation. |
Compressor cases | Heat and pressure-resistant. |
Machine parts | Precision components for various uses. |
Typical Uses of Aluminum 355.0 Sand Cast T6 | Typical Uses of Aluminum AlSi5Cu1Mg to ISO 3522 |