Designation

AISI 4130
ConditionNormalized
UNS numberG41300, ~H41300, ~K13047
US nameAMS 6345, AMS 6346, AMS 6348, AMS 6350, AMS 6356, AMS S 6758, AMS 6370, AMS 6371
EN name30CrMo4
EN number1.7216, 1.7220, 1.7221, 1.7226, 1.7230

AISI 4130, Low alloy steel, Normalized, Mechanical Properties

Young’s modulus200–210GPa
Specific stiffness25.5–26.9MN.m/kg
Yield strength (elastic limit)483–534MPa
Tensile strength621–686MPa
Specific strength61.6–68.2kN.m/kg
Elongation5–18% strain
Compressive strength483–534MPa
Flexural modulus200–210GPa
Flexural strength (modulus of rupture)483–534MPa
Shear modulus76–79.9GPa
Bulk modulus185–195GPa
Poisson’s ratio0.32–0.333 
Shape factor46   
Hardness – Vickers183–223HV
Elastic stored energy (springs)569–695kJ/m^3
Fatigue strength at 10^7 cycles299–347MPa
Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles279–372MPa

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey