AISI 4130, Low alloy steel, Annealed, Mechanical Properties

AISI 4130, Low alloy steel, Annealed, Mechanical Properties

Designation

AISI 4130
ConditionAnnealed
UNS numberG41300, ~H41300, ~K13047
US nameAMS 6345, AMS 6346, AMS 6348, AMS 6350, AMS 6356, AMS S 6758, AMS 6370, AMS 6371
EN name30CrMo4
EN number1.7216, 1.7220, 1.7221, 1.7226, 1.7230

AISI 4130, Low alloy steel, Annealed, Mechanical Properties

Young’s modulus201–216GPa
Specific stiffness25.6–27.5MN.m/kg
Yield strength (elastic limit)320–400MPa
Tensile strength500–620MPa
Specific strength40.8–51kN.m/kg
Elongation22–34% strain
Compressive strength320–400MPa
Flexural modulus201–216GPa
Flexural strength (modulus of rupture)320–400MPa
Shear modulus77–85GPa
Bulk modulus155–176GPa
Poisson’s ratio0.285–0.295 
Shape factor57   
Hardness – Vickers145–185HV
Hardness – Brinell148–164HB
Elastic stored energy (springs)248–381kJ/m^3
Fatigue strength at 10^7 cycles263–307MPa
Fatigue strength model (stress range)  227–355MPa

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey