ADI 1200 Composition

C (carbon)3.6–3.8%
Cu (copper)0–0.8%
Fe (iron)90.5–93.7%
Mn (manganese)0.26–0.3%
Mo (molybdenum)0–0.25%
Ni (nickel)0–2%
Si (silicon)2.4–2.8%

ADI 1200 Designation

ADI 1200
Condition                                                                                              Cast and austempered

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey