ADI 1200 Austempered Ductile Cast Iron Mechanical Properties
ADI 1200 Mechanical properties Young’s modulus 158 – 167 GPa Specific stiffness 22.3 – 23.6 MN.m/kg Yield strength (elastic limit) 900 – 1050 MPa Tensile strength 1200 – 1350 MPa Specific strength 127 – 148 kN.m/kg Elongation 3 – 7 % strain Compressive modulus 158 – 167 GPa Compressive strength 1.8e3 – 2.07e3 MPa Flexural … Continue reading ADI 1200 Austempered Ductile Cast Iron Mechanical Properties