| UNS number | F45009 |
Designation
BS EN 12513:2011 EN GJN HV600 (XCr23) (former BS 3D). Record based on BS 4844:1986 BS grade 3D
Standards with similar compositions:
| GB 8491(87) KmTBCr26 (China) |
| AFNOR NFA32401 FBCr26MoNi (France) |
| DIN G-X260Cr27 (Germany) |
| DIN G-X300CrMo271 (Germany) |
| DIN WNr 0.9650 (Germany) |
| DIN WNr 0.9655 (Germany) |
| IS 4771-3 HCr27/400 (India) |
| IS 4771-3 HCrNi27/400 (India) |
| SIS 140466 466 (Sweden) |
| BS 4844 3D (United Kingdom) |
| BS 4844 3E (United Kingdom) |
Typical uses
Abrasion resistant components, typically in mineral-pulverizing mills, e.g. grinding balls, drum liner plates, spiral classifier-shoes, pulverizing-bars.