AISI 1137 Resulfurized Medium Carbon Steel

AISI 1137 Resulfurized Medium Carbon Steel

AISI 1137 Steel Overview

AISI 1137 steel (UNS G11370) is a resulfurized medium carbon steel. AISI 1137 is a free-machining grade: its raised sulfur content gives short chips and fast cutting speeds. This page lists the AISI 1137 material data sheets for 13 conditions: annealed, as rolled, normalized, oil quenched & tempered at 205°C, oil quenched & tempered at 315°C, oil quenched & tempered at 425°C, oil quenched & tempered at 540°C, oil quenched & tempered at 650°C, water quenched & tempered at 205°C, water quenched & tempered at 315°C, water quenched & tempered at 425°C, water quenched & tempered at 540°C, water quenched & tempered at 650°C. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 1137 Steel

Heavy duty shafts, axles, crankshafts, couplings, used particularly where enhanced machinability is important.

AISI 1137 Steel Chemical Composition

C (carbon)0.32 – 0.39 %
Fe (iron)97.8 – 98.2 %
Mn (manganese)1.35 – 1.65 %
P (phosphorus)0 – 0.04 %
S (sulfur)0.08 – 0.13 %

AISI 1137 Steel Material Data Sheets

AISI 1137 Annealed Material Data Sheet

AISI 1137 As Rolled Material Data Sheet

AISI 1137 Normalized Material Data Sheet

AISI 1137 Oil Quenched & Tempered at 205°C Material Data Sheet

AISI 1137 Oil Quenched & Tempered at 315°C Material Data Sheet

AISI 1137 Oil Quenched & Tempered at 425°C Material Data Sheet

AISI 1137 Oil Quenched & Tempered at 540°C Material Data Sheet

AISI 1137 Oil Quenched & Tempered at 650°C Material Data Sheet

AISI 1137 Water Quenched & Tempered at 205°C Material Data Sheet

AISI 1137 Water Quenched & Tempered at 315°C Material Data Sheet

AISI 1137 Water Quenched & Tempered at 425°C Material Data Sheet

AISI 1137 Water Quenched & Tempered at 540°C Material Data Sheet

AISI 1137 Water Quenched & Tempered at 650°C Material Data Sheet

AISI 1137 Steel Condition Comparison

See how yield strength, tensile strength and hardness change between conditions in the AISI 1137 Annealed vs As Rolled vs Normalized vs Oil vs Water Quenched & Tempered (205–650°C): Yield, Tensile & Hardness Compared.

AISI 1137 Compared with Other Resulfurized Steels

Compare the composition, mechanical properties and machining speed of AISI 1137 with AISI 1117, 1118, 12L14, 1137, 1141 and 1144 in our resulfurized free-machining steels comparison.

AISI 1137 Steel Parts from Turkey

Looking for AISI 1137 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 1137 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all medium and high carbon steel grades.