AISI 1095 High Carbon Steel

AISI 1095 High Carbon Steel

AISI 1095 Steel Overview

AISI 1095 steel (UNS G10950) is a high carbon steel. This page lists the AISI 1095 material data sheets for 13 conditions: annealed, as rolled, normalized, oil quenched & tempered at 205°C, oil quenched & tempered at 315°C, oil quenched & tempered at 425°C, oil quenched & tempered at 540°C, oil quenched & tempered at 650°C, water quenched & tempered at 205°C, water quenched & tempered at 315°C, water quenched & tempered at 425°C, water quenched & tempered at 540°C, water quenched & tempered at 650°C. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 1095 Steel

General construction, general mechanical engineering, automotive, tools, axles, gears, springs.

AISI 1095 Steel Chemical Composition

C (carbon)0.9 – 1.03 %
Fe (iron)98.4 – 98.8 %
Mn (manganese)0.3 – 0.5 %
P (phosphorus)0 – 0.04 %
S (sulfur)0 – 0.05 %

AISI 1095 Steel Material Data Sheets

AISI 1095 Annealed Material Data Sheet

AISI 1095 As Rolled Material Data Sheet

AISI 1095 Normalized Material Data Sheet

AISI 1095 Oil Quenched & Tempered at 205°C Material Data Sheet

AISI 1095 Oil Quenched & Tempered at 315°C Material Data Sheet

AISI 1095 Oil Quenched & Tempered at 425°C Material Data Sheet

AISI 1095 Oil Quenched & Tempered at 540°C Material Data Sheet

AISI 1095 Oil Quenched & Tempered at 650°C Material Data Sheet

AISI 1095 Water Quenched & Tempered at 205°C Material Data Sheet

AISI 1095 Water Quenched & Tempered at 315°C Material Data Sheet

AISI 1095 Water Quenched & Tempered at 425°C Material Data Sheet

AISI 1095 Water Quenched & Tempered at 540°C Material Data Sheet

AISI 1095 Water Quenched & Tempered at 650°C Material Data Sheet

AISI 1095 Steel Condition Comparison

See how yield strength, tensile strength and hardness change between conditions in the AISI 1095 Annealed vs As Rolled vs Normalized vs Oil vs Water Quenched & Tempered (205–650°C): Yield, Tensile & Hardness Compared.