AISI 1015 Low Carbon Steel

AISI 1015 Low Carbon Steel

AISI 1015 Steel Overview

AISI 1015 steel (UNS G10150) is a low carbon steel. This page lists the AISI 1015 material data sheets for 3 conditions: annealed, as rolled, normalized. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 1015 Steel

General construction, general mechanical engineering, automotive, tools, axles, gears, springs.

AISI 1015 Steel Chemical Composition

C (carbon)0.13 – 0.18 %
Fe (iron)99.1 – 99.6 %
Mn (manganese)0.3 – 0.6 %
P (phosphorus)0 – 0.04 %
S (sulfur)0 – 0.05 %

AISI 1015 Steel Material Data Sheets

AISI 1015 Annealed Material Data Sheet

AISI 1015 As Rolled Material Data Sheet

AISI 1015 Normalized Material Data Sheet

AISI 1015 Steel Condition Comparison

See how yield strength, tensile strength and hardness change between conditions in the AISI 1015 Annealed vs As Rolled vs Normalized: Yield, Tensile & Hardness Compared.