PA410 Impact Modified Grade (Polyamide 410) Material Data Sheet
PA410 Impact Modified Grade Overview
PA410 impact modified grade is a grade of polyamide 410 (PA410, nylon 410), designated Polyamide (Nylon) (Type 410, impact modified). This PA410 impact modified grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA410 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA410 parts in-house and inspects them before shipment.
PA410 Impact Modified Grade Designation
Polyamide (Nylon) (Type 410, impact modified) Tradenames EcoPaXX®
PA410 Impact Modified Grade Typical uses
General purpose, automotive parts, engine covers, fuel tanks, tubing, wheels, household goods, sporting goods, electrical components
PA410 Impact Modified Grade Composition detail
Polymer 85 – 95 % Impact modifier 5 – 15 %
PA410 Impact Modified Grade Physical properties
PA410 Impact Modified Grade Mechanical properties
Young’s modulus 0.9 – 0.946 GPa Specific stiffness 0.856 – 0.902 MN.m/kg Yield strength (elastic limit) 35 – 40.8 MPa Tensile strength 35 – 40.8 MPa Specific strength 33.3 – 38.9 kN.m/kg Elongation 50 – 72 % strain Elongation at yield 20 – 28.8 % strain Compressive modulus 0.9 – 0.945 GPa Compressive strength 35 – 40.8 MPa Flexural modulus 0.95 – 0.998 GPa Flexural strength (modulus of rupture) 40 – 46.7 MPa Shear modulus 0.9 – 0.945 GPa Shear strength 21 – 24.5 MPa Bulk modulus 1.01 – 1.03 GPa Poisson’s ratio 0.34 – 0.36 Shape factor 1.94 Hardness – Vickers 11 – 12 HV Hardness – Shore D 72 – 78 Elastic stored energy (springs) 666 – 899 kJ/m3 Fatigue strength at 10^7 cycles 14 – 16.3 MPa
PA410 Impact Modified Grade Impact & fracture properties
Fracture toughness 2.88 – 3.48 MPa.m0.5 Toughness (G) 9.05 – 13 kJ/m2 Impact strength, notched 23 °C 62 – 75 kJ/m2 Impact strength, notched -30 °C 9 – 20 kJ/m2 Impact strength, unnotched 23 °C 590 – 600 kJ/m2 Impact strength, unnotched -30 °C 590 – 600 kJ/m2
PA410 Impact Modified Grade Thermal properties
Melting point 250 °C Glass temperature 52.3 – 66.3 °C Heat deflection temperature 0.45MPa 140 – 164 °C Heat deflection temperature 1.8MPa 65.5 – 85.5 °C Vicat softening point 157 – 182 °C Maximum service temperature 192 – 210 °C Minimum service temperature -64 – -54 °C Thermal conductivity 0.231 – 0.25 W/m.°C Specific heat capacity 1370 – 1430 J/kg.°C Thermal expansion coefficient 120 – 140 µstrain/°C Thermal shock resistance 283 – 353 °C Thermal distortion resistance 0.0017 – 0.00202 MW/m
PA410 Impact Modified Grade Electrical properties
Electrical resistivity 9.09e19 – 1.1e20 µohm.cm Electrical conductivity 1.57e-18 – 1.9e-18 %IACS Dielectric constant (relative permittivity) 5.16 – 5.59 Dissipation factor (dielectric loss tangent) 0.208 – 0.3 Dielectric strength (dielectric breakdown) 28.6 – 31.5 MV/m Comparative tracking index 571 – 630 V
PA410 Impact Modified Grade Magnetic properties
Magnetic type Non-magnetic
PA410 Impact Modified Grade Optical, aesthetic and acoustic properties
Transparency Transparent Acoustic velocity 925 – 950 m/s Mechanical loss coefficient (tan delta) 0.024 – 0.0317
PA410 Impact Modified Grade Absorption & permeability
Water absorption @ 24 hrs 0.455 – 0.55 % Water absorption @ sat 5.27 – 6.38 % Humidity absorption @ sat 1.55 – 1.87 % Water vapor transmission 0.865 – 1.46 g.mm/m².day Permeability (O2) 0.339 – 0.995 cm³.mm/m².day.atm
PA410 Impact Modified Grade Processing properties
First commercial production 2010 Polymer injection molding Excellent Polymer extrusion Acceptable Polymer thermoforming Limited use Linear mold shrinkage 1 – 1.2 % Melt temperature 270 – 300 °C Mold temperature 60 – 100 °C
PA410 Impact Modified Grade Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Acceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Limited use Organic solvents Excellent Oils and fuels Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Slow-burning
PA410 Impact Modified Grade Notes
PA410 Impact Modified Grade Other notes Polyamide 410 is 70% derived from castor oil. It has excellent mechanical properties, high heat stability and outstanding chemical resistance. Polyamide 410 also offers low permeability to both oxygen and water vapor; and and low moisture absorption for improved dimensional stability post conditioning.