PA1010 (Polyamide 1010 / Nylon 1010)

PA1010 (Polyamide 1010 / Nylon 1010)

PA1010 Overview

PA1010 (nylon 1010) is a long-chain polyamide made from decamethylene diamine and sebacic acid, both of which can be produced from castor oil, so it can be fully bio-based. Like other long-chain polyamides it absorbs less water than PA6 or PA66, which helps dimensional stability, and it offers good chemical resistance and toughness. It is used for molded and extruded parts such as tubing, connectors and technical components.

PA1010 Parts from Turkey

Looking for PA1010 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA1010 parts in-house and inspects them before shipment.

PA1010 Grades

PA1010 Unfilled Grades

PA1010 Molding and Extrusion Material Data Sheet