PA1010 Molding and Extrusion Material Data Sheet

PA1010 Molding and Extrusion (Polyamide 1010) Material Data Sheet

PA1010 Molding and Extrusion Overview

PA1010 molding and extrusion is a grade of polyamide 1010 (PA1010, nylon 1010), designated Polyamide (Nylon) (Type 1010, molding and extrusion). This PA1010 molding and extrusion material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA1010 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA1010 parts in-house and inspects them before shipment.

PA1010 Molding and Extrusion Designation

Polyamide (Nylon) (Type 1010, molding and extrusion)
TradenamesGrilamid, Hiprolon, Terez, Vestamid, Zytel

PA1010 Molding and Extrusion Composition detail

Polymer100  %

PA1010 Molding and Extrusion Physical properties

Density1.05–1.08g/cm3

PA1010 Molding and Extrusion Mechanical properties

Young’s modulus1.16–1.2GPa
Specific stiffness1.08–1.13MN.m/kg
Yield strength (elastic limit)45–49MPa
Tensile strength47–51MPa
Specific strength42.2–46.1kN.m/kg
Elongation210  % strain
Elongation at yield24  % strain
Compressive modulus1.16–1.2GPa
Compressive strength56.4–61.2MPa
Flexural modulus1.16–1.2GPa
Flexural strength (modulus of rupture)70–75MPa
Shear modulus0.413–0.422GPa
Shear strength28.2–30.6MPa
Bulk modulus2.06–2.6GPa
Poisson’s ratio0.406–0.423 
Shape factor3.8
Hardness – Vickers10–11HV
Hardness – Rockwell M70–80 
Hardness – Rockwell R100–110 
Hardness – Shore D77–78 
Elastic stored energy (springs)858–1020kJ/m3
Fatigue strength at 10^7 cycles18.8–20.4MPa

PA1010 Molding and Extrusion Impact & fracture properties

Fracture toughness3.32–3.34MPa.m0.5
Toughness (G)9.23–9.57kJ/m2
Impact strength, notched 23 °C10  kJ/m2
Impact strength, notched -30 °C5  kJ/m2
Impact strength, unnotched 23 °C590–600kJ/m2
Impact strength, unnotched -30 °C590–600kJ/m2

PA1010 Molding and Extrusion Thermal properties

Melting point200–203°C
Glass temperature37  °C
Heat deflection temperature 0.45MPa101–110°C
Heat deflection temperature 1.8MPa55  °C
Vicat softening point171  °C
Maximum service temperature80–110°C
Minimum service temperature-50–-40°C
Thermal conductivity0.2–0.3W/m.°C
Specific heat capacity1700–1750J/kg.°C
Thermal expansion coefficient120–140µstrain/°C
Thermal shock resistance281–336°C
Thermal distortion resistance0.00153–0.00234MW/m

PA1010 Molding and Extrusion Electrical properties

Electrical resistivity1e18–1e19µohm.cm
Electrical conductivity1.72e-17–1.72e-16%IACS
Dielectric constant (relative permittivity)5–6 
Dissipation factor (dielectric loss tangent)0.07–0.15 
Dielectric strength (dielectric breakdown)20–30MV/m
Comparative tracking index600  V

PA1010 Molding and Extrusion Magnetic properties

Magnetic typeNon-magnetic

PA1010 Molding and Extrusion Optical, aesthetic and acoustic properties

TransparencyTranslucent
Acoustic velocity1040–1060m/s
Mechanical loss coefficient (tan delta)0.0242–0.0246 

PA1010 Molding and Extrusion Absorption & permeability

Water absorption @ 24 hrs0.5–0.8%
Water absorption @ sat1.8  %
Humidity absorption @ sat0.6–0.8%

PA1010 Molding and Extrusion Processing properties

Polymer injection moldingAcceptable
Polymer extrusionAcceptable
Polymer thermoformingLimited use
Linear mold shrinkage1 – 2 %

PA1010 Molding and Extrusion Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisExcellent
Strong alkalisLimited use
Organic solventsAcceptable
Oils and fuelsAcceptable
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySlow-burning

PA1010 Molding and Extrusion Notes

PA1010 Molding and Extrusion Other notes
PA type 1010 is 100% bio-based, derived from castor oil (a vegetable oil extracted from castor seeds) as its main chemical feedstock