Home » PA (Polyamide / Nylon) » PA69 (Polyamide 69 / Nylon 69) » PA69 Unfilled Grades » PA69 Unfilled Grade Material Data Sheet
PA69 Unfilled Grade (Polyamide 69) Material Data Sheet
PA69 Unfilled Grade Overview
PA69 unfilled grade is a grade of polyamide 69 (PA69, nylon 69), designated Polyamide (Nylon) (Type 69, Molding and Extrusion). This PA69 unfilled grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA69 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA69 parts in-house and inspects them before shipment.
PA69 Unfilled Grade Designation
Polyamide (Nylon) (Type 69, Molding and Extrusion) Tradenames Amilan; Antron; Aquanyl; Aramica; Ascend; Badamid; Bergamid; Bestnyl; Cordura; Dynacom; Emarex; Emmon; Ensiln; Ertalon; Esbrid; Estomid; Fostalink; Gapex; Grivory; Hiloy; Kobatron; Lubrilon; Lupon; Macromelt; Malecca; MCX-Q; NewNalon; Novamid; NSC; Nycast; Nylamid; Nylene; Nyloil; Nylube; Oilon; Oromid; Palmid; Polyslider; Ponamid; Pyronyl; Radiflam; Rayfan; Selar; Shinite; Spylon; StaMax; Starflam; Sunmide; Supplex; Tecast; Technystar; Terez; Texalon; Tismo Poticon; Trogamid; Tynex; Ultramid; Vekton; Wellamid; XTI; Zytel
PA69 Unfilled Grade Typical uses
General mechanical parts as for Nylon 6 or Nylon 66, but which require better dimensional stability.
PA69 Unfilled Grade Composition detail
PA69 Unfilled Grade Physical properties
PA69 Unfilled Grade Mechanical properties
Young’s modulus 1.85 – 1.94 GPa Specific stiffness 1.69 – 1.78 MN.m/kg Yield strength (elastic limit) 44.6 – 49.2 MPa Tensile strength 55.8 – 61.5 MPa Specific strength 40.9 – 45.2 kN.m/kg Elongation 1050 – 1210 % strain Compressive modulus 1.85 – 1.94 GPa Compressive strength 66.8 – 73.8 MPa Flexural modulus 1.95 – 2.04 GPa Flexural strength (modulus of rupture) 78.1 – 86.1 MPa Shear modulus 0.658 – 0.69 GPa Bulk modulus 3.24 – 3.4 GPa Poisson’s ratio 0.397 – 0.413 Shape factor 4.7 Hardness – Vickers 13 – 15 HV Hardness – Rockwell M 71 – 78 Hardness – Rockwell R 106 – 117 Elastic stored energy (springs) 526 – 639 kJ/m3 Fatigue strength at 10^7 cycles 20.6 – 26.7 MPa
PA69 Unfilled Grade Impact & fracture properties
Fracture toughness 1.59 – 2.32 MPa.m0.5 Toughness (G) 1.37 – 2.77 kJ/m2 Impact strength, notched 23 °C 5.5 – 6.1 kJ/m2
PA69 Unfilled Grade Thermal properties
Melting point 196 – 215 °C Glass temperature 54 – 62 °C Heat deflection temperature 0.45MPa 166 – 171 °C Heat deflection temperature 1.8MPa 57 – 60 °C Maximum service temperature 90 – 130 °C Minimum service temperature -62 – -42 °C Thermal conductivity 0.239 – 0.249 W/m.°C Specific heat capacity 1500 – 1540 J/kg.°C Thermal expansion coefficient 89.1 – 90.9 µstrain/°C Thermal shock resistance 260 – 290 °C Thermal distortion resistance 0.00265 – 0.00277 MW/m
PA69 Unfilled Grade Electrical properties
Electrical resistivity 1e19 – 1e21 µohm.cm Electrical conductivity 1.72e-19 – 1.72e-17 %IACS Dielectric constant (relative permittivity) 5.12 – 5.63 Dissipation factor (dielectric loss tangent) 0.019 – 0.021 Dielectric strength (dielectric breakdown) 22.7 – 24.6 MV/m Comparative tracking index 250 – 600 V
PA69 Unfilled Grade Magnetic properties
Magnetic type Non-magnetic
PA69 Unfilled Grade Optical, aesthetic and acoustic properties
Transparency Translucent Acoustic velocity 1300 – 1340 m/s Mechanical loss coefficient (tan delta) 0.0206 – 0.0216
PA69 Unfilled Grade Absorption & permeability
Water absorption @ 24 hrs 0.455 – 0.55 %
PA69 Unfilled Grade Processing properties
Polymer injection molding Limited use Polymer extrusion Acceptable Polymer thermoforming Limited use Linear mold shrinkage 1 – 1.5 % Melt temperature 218 – 260 °C Mold temperature 40 – 80 °C Molding pressure range 6.88 – 103 MPa
PA69 Unfilled Grade Durability
Water (fresh) Acceptable Water (salt) Acceptable Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Limited use Strong alkalis Unacceptable Organic solvents Acceptable Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Slow-burning
PA69 Grades
PA69 Unfilled Material Data Sheets
Unfilled Unfilled You are here
Other PA69 grades:
All PA69 Grades
Modulus Metal Services
Manufacturing & Quality Services in Turkey