PA612 30% Carbon Fiber 10% PTFE Lubricated Material Data Sheet

PA612 30% Carbon Fiber 10% PTFE Lubricated (Polyamide 612) Material Data Sheet

PA612 30% Carbon Fiber 10% PTFE Lubricated Overview

PA612 30% carbon fiber 10% PTFE lubricated is a grade of polyamide 612 (PA612, nylon 612), designated Polyamide (Nylon) (Type 612, 30% carbon fiber, 10% PTFE, lubricated). This PA612 30% carbon fiber 10% PTFE lubricated material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA612 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA612 parts in-house and inspects them before shipment.

PA612 30% Carbon Fiber 10% PTFE Lubricated Designation

Polyamide (Nylon) (Type 612, 30% carbon fiber, 10% PTFE, lubricated)
TradenamesInlube, Lubrione, Tribocomp

PA612 30% Carbon Fiber 10% PTFE Lubricated Typical uses

Mechanical parts, zips, filaments, coverings and coatings requiring abrasion resistance.

PA612 30% Carbon Fiber 10% PTFE Lubricated Composition detail

Polymer60  %
PTFE (lubricant)10  %
Carbon (fiber)30  %

PA612 30% Carbon Fiber 10% PTFE Lubricated Physical properties

Density1.31–1.34g/cm3

PA612 30% Carbon Fiber 10% PTFE Lubricated Mechanical properties

Young’s modulus16–19.9GPa
Specific stiffness12.1–15MN.m/kg
Yield strength (elastic limit)174–217MPa
Tensile strength176–215MPa
Specific strength131–164kN.m/kg
Elongation1.83–2.63% strain
Elongation at yield1.54–2.92% strain
Compressive modulus17.1–18.9GPa
Compressive strength223–246MPa
Flexural modulus13.8–16.5GPa
Flexural strength (modulus of rupture)268–328MPa
Shear modulus6.54–6.88GPa
Shear strength106–129MPa
Bulk modulus17.6–19.4GPa
Poisson’s ratio0.325–0.338 
Shape factor7.73
Hardness – Vickers56–62HV
Hardness – Rockwell M184–204 
Hardness – Rockwell R184–204 
Hardness – Shore D98–102 
Elastic stored energy (springs)839–1330kJ/m3
Fatigue strength at 10^7 cycles74.3–82.1MPa

PA612 30% Carbon Fiber 10% PTFE Lubricated Impact & fracture properties

Fracture toughness5.48–6.06MPa.m0.5
Toughness (G)1.61–2.15kJ/m2
Impact strength, notched 23 °C10.2–19.8kJ/m2
Impact strength, notched -30 °C6.3–13.7kJ/m2
Impact strength, unnotched 23 °C64.8–95.2kJ/m2
Impact strength, unnotched -30 °C42–63kJ/m2

PA612 30% Carbon Fiber 10% PTFE Lubricated Thermal properties

Melting point195–217°C
Glass temperature40–52°C
Heat deflection temperature 0.45MPa201–249°C
Heat deflection temperature 1.8MPa176–222°C
Maximum service temperature90–120°C
Minimum service temperature-127–-107°C
Thermal conductivity0.57–0.593W/m.°C
Specific heat capacity1450–1510J/kg.°C
Thermal expansion coefficient30.1–30.7µstrain/°C
Thermal shock resistance308–417°C
Thermal distortion resistance0.0187–0.0196MW/m

PA612 30% Carbon Fiber 10% PTFE Lubricated Electrical properties

Electrical resistivity100000–1e7µohm.cm
Electrical conductivity1.72e-5–0.00172%IACS
Galvanic potential0.14–0.22V

PA612 30% Carbon Fiber 10% PTFE Lubricated Magnetic properties

Magnetic typeNon-magnetic

PA612 30% Carbon Fiber 10% PTFE Lubricated Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity3470–3880m/s
Mechanical loss coefficient (tan delta)0.00645–0.00713 

PA612 30% Carbon Fiber 10% PTFE Lubricated Absorption & permeability

Water absorption @ 24 hrs0.3–0.48%
Water absorption @ sat1.3–1.7%
Humidity absorption @ sat0.55–0.75%

PA612 30% Carbon Fiber 10% PTFE Lubricated Processing properties

Polymer injection moldingLimited use
Polymer extrusionUnsuitable
Polymer thermoformingLimited use
Linear mold shrinkage0.118 – 0.143 %
Melt temperature213 – 288 °C
Mold temperature30 – 60 °C
Molding pressure range27.5 – 138 MPa

PA612 30% Carbon Fiber 10% PTFE Lubricated Durability

Water (fresh)Acceptable
Water (salt)Acceptable
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisAcceptable
Organic solventsAcceptable
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySlow-burning