PA610 Unfilled Grade Material Data Sheet

PA610 Unfilled Grade (Polyamide 610) Material Data Sheet

PA610 Unfilled Grade Overview

PA610 unfilled grade is a grade of polyamide 610 (PA610, nylon 610), designated Polyamide (Nylon) (Type 610, Molding and Extrusion). This PA610 unfilled grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA610 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA610 parts in-house and inspects them before shipment.

PA610 Unfilled Grade Designation

Polyamide (Nylon) (Type 610, Molding and Extrusion)
TradenamesAkromid, Amilan, Badamid, Grilamid, Hiprolon, Isocor, Nylene, Shandong, Technyl Exten, Terez, Ultramid, Vestamid, Zytel

PA610 Unfilled Grade Typical uses

Zip fasteners, electrical insulators, precision parts, filaments for brushes.

PA610 Unfilled Grade Composition detail

Polymer100  %

PA610 Unfilled Grade Physical properties

Density1.06–1.08g/cm3

PA610 Unfilled Grade Mechanical properties

Young’s modulus1.45–1.8GPa
Specific stiffness1.35–1.68MN.m/kg
Yield strength (elastic limit)44.5–55.5MPa
Tensile strength56.6–69.2MPa
Specific strength41.6–51.9kN.m/kg
Elongation41–59% strain
Elongation at yield15.2–28.8% strain
Compressive modulus1.54–1.71GPa
Compressive strength71.7–79.3MPa
Flexural modulus1.48–1.77GPa
Flexural strength (modulus of rupture)75.7–92.5MPa
Shear modulus0.566–0.595GPa
Shear strength34–41.5MPa
Bulk modulus2.57–2.84GPa
Poisson’s ratio0.35–0.4 
Shape factor4.3
Hardness – Vickers14–16HV
Hardness – Rockwell M114–126 
Hardness – Rockwell R114–126 
Hardness – Shore D81–84 
Elastic stored energy (springs)607–963kJ/m3
Fatigue strength at 10^7 cycles23.9–26.4MPa

PA610 Unfilled Grade Impact & fracture properties

Fracture toughness3.37–3.73MPa.m0.5
Toughness (G)6.74–8.98kJ/m2
Impact strength, notched 23 °C5.57–10.8kJ/m2
Impact strength, unnotched 23 °C590–600kJ/m2
Impact strength, unnotched -30 °C590–600kJ/m2

PA610 Unfilled Grade Thermal properties

Melting point210–230°C
Glass temperature44–56°C
Heat deflection temperature 0.45MPa157–173°C
Heat deflection temperature 1.8MPa76–84°C
Maximum service temperature90–120°C
Minimum service temperature-64–-44°C
Thermal conductivity0.2–0.22W/m.°C
Specific heat capacity1540–1590J/kg.°C
Thermal expansion coefficient139–141µstrain/°C
Thermal shock resistance189–256°C
Thermal distortion resistance0.00143–0.00157MW/m

PA610 Unfilled Grade Electrical properties

Electrical resistivity1.32e19–3.3e20µohm.cm
Electrical conductivity5.22e-19–1.31e-17%IACS
Dielectric constant (relative permittivity)4.26–6.01 
Dissipation factor (dielectric loss tangent)0.0431–0.114 
Dielectric strength (dielectric breakdown)23.5–40.1MV/m
Comparative tracking index600  V

PA610 Unfilled Grade Magnetic properties

Magnetic typeNon-magnetic

PA610 Unfilled Grade Optical, aesthetic and acoustic properties

Refractive index1.56–1.57 
TransparencyTranslucent
Acoustic velocity1160–1300m/s
Mechanical loss coefficient (tan delta)0.0197–0.0218 

PA610 Unfilled Grade Absorption & permeability

Water absorption @ 24 hrs0.78–1.3%
Water absorption @ sat3.4–4.6%
Humidity absorption @ sat1.2–1.6%

PA610 Unfilled Grade Processing properties

Polymer injection moldingExcellent
Polymer extrusionAcceptable
Polymer thermoformingLimited use
Linear mold shrinkage0.5 – 1.5 %
Melt temperature229 – 260 °C
Mold temperature30 – 60 °C
Molding pressure range6.88 – 131 MPa

PA610 Unfilled Grade Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisAcceptable
Organic solventsAcceptable
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySlow-burning