Home » PA (Polyamide / Nylon) » PA46 (Polyamide 46 / Nylon 46) » PA46 Unfilled Grades » PA46 Super-Tough Grade Material Data Sheet
PA46 Super-Tough Grade (Polyamide 46) Material Data Sheet
PA46 Super-Tough Grade Overview
PA46 super-tough grade is a grade of polyamide 46 (PA46, nylon 46), designated Polyamide (Nylon) (Type 46, Super-tough). This PA46 super-tough grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA46 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA46 parts in-house and inspects them before shipment.
PA46 Super-Tough Grade Designation
Polyamide (Nylon) (Type 46, Super-tough) Tradenames Stanyl
PA46 Super-Tough Grade Typical uses
Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.
PA46 Super-Tough Grade Composition detail
Polymer 75 – 80 % Impact modifier 20 – 25 %
PA46 Super-Tough Grade Physical properties
PA46 Super-Tough Grade Mechanical properties
Young’s modulus 0.534 – 0.666 GPa Specific stiffness 0.487 – 0.609 MN.m/kg Yield strength (elastic limit) 40.1 – 50 MPa Tensile strength 41.3 – 50.5 MPa Specific strength 36.6 – 45.7 kN.m/kg Elongation 29.3 – 42.2 % strain Elongation at yield 17.3 – 32.8 % strain Compressive modulus 0.57 – 0.63 GPa Compressive strength 52.1 – 57.5 MPa Flexural modulus 0.501 – 0.6 GPa Flexural strength (modulus of rupture) 36 – 44 MPa Shear modulus 0.207 – 0.217 GPa Shear strength 24.8 – 30.3 MPa Bulk modulus 1.12 – 1.24 GPa Poisson’s ratio 0.399 – 0.415 Shape factor 3.1 Hardness – Vickers 13 – 14 HV Hardness – Rockwell M 95 – 105 Hardness – Rockwell R 95 – 105 Hardness – Shore D 75 – 79 Elastic stored energy (springs) 1330 – 2120 kJ/m3 Fatigue strength at 10^7 cycles 17.4 – 19.3 MPa
PA46 Super-Tough Grade Impact & fracture properties
Fracture toughness 2.76 – 3.05 MPa.m0.5 Toughness (G) 12.2 – 16.3 kJ/m2 Impact strength, notched 23 °C 88.4 – 172 kJ/m2 Impact strength, notched -30 °C 18.9 – 41.1 kJ/m2 Impact strength, unnotched 23 °C 590 – 600 kJ/m2 Impact strength, unnotched -30 °C 590 – 600 kJ/m2
PA46 Super-Tough Grade Thermal properties
Melting point 284 – 306 °C Glass temperature 71 – 79 °C Heat deflection temperature 0.45MPa 98 – 135 °C Heat deflection temperature 1.8MPa 73 – 108 °C Maximum service temperature 73 – 87 °C Minimum service temperature -58 – -38 °C Thermal conductivity 0.233 – 0.242 W/m.°C Specific heat capacity 1630 – 1700 J/kg.°C Thermal expansion coefficient 142 – 145 µstrain/°C Thermal shock resistance 449 – 609 °C Thermal distortion resistance 0.00162 – 0.00169 MW/m
PA46 Super-Tough Grade Electrical properties
Electrical resistivity 2e14 – 5e15 µohm.cm Electrical conductivity 3.45e-14 – 8.62e-13 %IACS Dielectric constant (relative permittivity) 11.6 – 16.4 Dissipation factor (dielectric loss tangent) 0.358 – 0.943 Dielectric strength (dielectric breakdown) 11.1 – 18.9 MV/m Comparative tracking index 475 – 525 V
PA46 Super-Tough Grade Magnetic properties
Magnetic type Non-magnetic
PA46 Super-Tough Grade Optical, aesthetic and acoustic properties
Refractive index 1.62 – 1.64 Transparency Opaque Acoustic velocity 697 – 781 m/s Mechanical loss coefficient (tan delta) 0.0339 – 0.0375
PA46 Super-Tough Grade Absorption & permeability
Water absorption @ 24 hrs 2.3 – 3.7 % Water absorption @ sat 9.5 – 13 % Humidity absorption @ sat 2.5 – 3.4 %
PA46 Super-Tough Grade Processing properties
Polymer injection molding Acceptable Polymer extrusion Acceptable Polymer thermoforming Limited use Linear mold shrinkage 1.8 – 2 % Melt temperature 242 – 316 °C Mold temperature 40 – 80 °C Molding pressure range 34.4 – 103 MPa
PA46 Super-Tough Grade Durability
Water (fresh) Acceptable Water (salt) Acceptable Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Unacceptable Organic solvents Acceptable Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Slow-burning