Home » PA (Polyamide / Nylon) » PA66 (Polyamide 66 / Nylon 66) » PA66 Glass and Mineral Filled Grades » PA66 40% Glass and Mineral Material Data Sheet
PA66 40% Glass and Mineral (Polyamide 66) Material Data Sheet
PA66 40% Glass and Mineral Overview
PA66 40% glass and mineral is a grade of polyamide 66 (PA66, nylon 66), designated Polyamide (Nylon) (Type 66, 40% Glass and Mineral). This PA66 40% glass and mineral material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.
PA66 40% Glass and Mineral Designation
Polyamide (Nylon) (Type 66, 40% Glass and Mineral) Tradenames Akulon, Alcom, Bestnyl, Chemlon, Clariant, Durethan, Ecolon, Hifill, Hylon, Kepamid, Maxamid, Minlon, Nybex, Scanamid, Schulamid, Technyl, Tekamid, Ultramid, Wellamid
PA66 40% Glass and Mineral Typical uses
Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.
PA66 40% Glass and Mineral Composition detail
Polymer 60 % Glass (fiber) 15 – 25 % Mineral (unspecified) 15 – 25 %
PA66 40% Glass and Mineral Physical properties
PA66 40% Glass and Mineral Mechanical properties
Young’s modulus 5.11 – 6.38 GPa Specific stiffness 3.49 – 4.36 MN.m/kg Yield strength (elastic limit) 74 – 92.3 MPa Tensile strength 74.9 – 91.5 MPa Specific strength 50.5 – 63 kN.m/kg Elongation 4.98 – 7.16 % strain Elongation at yield 4.19 – 7.95 % strain Compressive modulus 5.46 – 6.03 GPa Compressive strength 94.8 – 105 MPa Flexural modulus 4.83 – 5.78 GPa Flexural strength (modulus of rupture) 111 – 135 MPa Shear modulus 2.05 – 2.15 GPa Shear strength 44.9 – 54.9 MPa Bulk modulus 6.89 – 7.62 GPa Poisson’s ratio 0.347 – 0.368 Shape factor 6.42 Hardness – Vickers 24 – 26 HV Hardness – Rockwell M 132 – 146 Hardness – Rockwell R 132 – 146 Hardness – Shore D 86 – 89 Elastic stored energy (springs) 474 – 755 kJ/m3 Fatigue strength at 10^7 cycles 31.6 – 34.9 MPa
PA66 40% Glass and Mineral Impact & fracture properties
Fracture toughness 4.35 – 4.81 MPa.m0.5 Toughness (G) 3.17 – 4.24 kJ/m2 Impact strength, notched 23 °C 4.61 – 8.94 kJ/m2 Impact strength, notched -30 °C 2.29 – 4.98 kJ/m2 Impact strength, unnotched 23 °C 40.1 – 58.9 kJ/m2 Impact strength, unnotched -30 °C 30 – 45 kJ/m2
PA66 40% Glass and Mineral Thermal properties
Melting point 250 – 260 °C Glass temperature 54 – 66 °C Heat deflection temperature 0.45MPa 249 – 258 °C Heat deflection temperature 1.8MPa 222 – 252 °C Maximum service temperature 90 – 130 °C Minimum service temperature -81 – -71 °C Thermal conductivity 0.443 – 0.479 W/m.°C Specific heat capacity 1320 – 1380 J/kg.°C Thermal expansion coefficient 36 – 97.2 µstrain/°C Thermal shock resistance 147 – 407 °C Thermal distortion resistance 0.00474 – 0.0128 MW/m
PA66 40% Glass and Mineral Electrical properties
Electrical resistivity 2.87e19 – 7.18e20 µohm.cm Electrical conductivity 2.4e-19 – 6.01e-18 %IACS Dielectric constant (relative permittivity) 9.96 – 14 Dissipation factor (dielectric loss tangent) 0.127 – 0.334 Dielectric strength (dielectric breakdown) 25.9 – 44.1 MV/m Comparative tracking index 375 – 450 V
PA66 40% Glass and Mineral Magnetic properties
Magnetic type Non-magnetic
PA66 40% Glass and Mineral Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 1860 – 2090 m/s Mechanical loss coefficient (tan delta) 0.0109 – 0.0121
PA66 40% Glass and Mineral Absorption & permeability
Water absorption @ 24 hrs 0.46 – 0.74 % Water absorption @ sat 4.3 – 5.7 % Humidity absorption @ sat 1.2 – 1.7 %
PA66 40% Glass and Mineral Processing properties
Polymer injection molding Excellent Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.1 – 0.5 % Melt temperature 223 – 310 °C Molding pressure range 61.9 – 138 MPa
PA66 40% Glass and Mineral Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Acceptable Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Poor Flammability Slow-burning
PA66 Grades
PA66 Glass and Mineral Filled Material Data Sheets
Glass+Min 40% Glass and Mineral You are here
All PA66 Grades
Modulus Metal Services
Manufacturing & Quality Services in Turkey