PA6/66 Copolymer Grade Material Data Sheet

PA6/66 Copolymer Grade (Polyamide 6/66) Material Data Sheet

PA6/66 Copolymer Grade Overview

PA6/66 copolymer grade is a grade of polyamide 6/66 (PA6/66, nylon 6/66), designated Polyamide (Nylon) (Type 66/6). This PA6/66 copolymer grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA6/66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA6/66 parts in-house and inspects them before shipment.

PA6/66 Copolymer Grade Designation

Polyamide (Nylon) (Type 66/6)
TradenamesGrilon, Pentamid, Technyl, Vitamide, Yuyao

PA6/66 Copolymer Grade Typical uses

Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.

PA6/66 Copolymer Grade Composition detail

Polymer75–85%
Impact modifier15–25%

PA6/66 Copolymer Grade Physical properties

Density1.08–1.1g/cm3

PA6/66 Copolymer Grade Mechanical properties

Young’s modulus0.691–0.862GPa
Specific stiffness0.634–0.791MN.m/kg
Yield strength (elastic limit)28.6–35.7MPa
Tensile strength36.2–44.2MPa
Specific strength26.2–32.8kN.m/kg
Elongation41–59% strain
Elongation at yield10.9–20.8% strain
Compressive modulus0.738–0.816GPa
Compressive strength45.8–50.6MPa
Flexural modulus0.707–0.847GPa
Flexural strength (modulus of rupture)43.5–53.1MPa
Shear modulus0.278–0.293GPa
Shear strength21.7–26.5MPa
Bulk modulus0.879–0.971GPa
Poisson’s ratio0.34–0.36 
Shape factor3.8
Hardness – Vickers9–10HV
Hardness – Rockwell M88–97 
Hardness – Rockwell R88–97 
Hardness – Shore D73–76 
Elastic stored energy (springs)524–835kJ/m3
Fatigue strength at 10^7 cycles15.3–16.9MPa

PA6/66 Copolymer Grade Impact & fracture properties

Fracture toughness2.91–3.21MPa.m0.5
Toughness (G)10.5–14kJ/m2
Impact strength, notched 23 °C114–221kJ/m2
Impact strength, notched -30 °C3.06–6.64kJ/m2
Impact strength, unnotched 23 °C590–600kJ/m2
Impact strength, unnotched -30 °C247–371kJ/m2

PA6/66 Copolymer Grade Thermal properties

Melting point210–220°C
Glass temperature44–56°C
Heat deflection temperature 0.45MPa127–186°C
Heat deflection temperature 1.8MPa45–60°C
Maximum service temperature52–67°C
Minimum service temperature-64–-54°C
Thermal conductivity0.216–0.224W/m.°C
Specific heat capacity1610–1680J/kg.°C
Thermal expansion coefficient130–216µstrain/°C
Thermal shock resistance185–330°C
Thermal distortion resistance0.00102–0.0017MW/m

PA6/66 Copolymer Grade Electrical properties

Electrical resistivity3.32e19–8.3e20µohm.cm
Electrical conductivity2.08e-19–5.19e-18%IACS
Dielectric constant (relative permittivity)7.47–10.5 
Dissipation factor (dielectric loss tangent)0.055–0.145 
Dielectric strength (dielectric breakdown)20.9–35.5MV/m
Comparative tracking index600  V

PA6/66 Copolymer Grade Magnetic properties

Magnetic typeNon-magnetic

PA6/66 Copolymer Grade Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity795–891m/s
Mechanical loss coefficient (tan delta)0.0285–0.0315 

PA6/66 Copolymer Grade Absorption & permeability

Water absorption @ 24 hrs1.7–2.7%
Water absorption @ sat7.3–9.7%
Humidity absorption @ sat2.3–3.1%
Water vapor transmission0.958–1.73g.mm/m².day
Permeability (O2)0.622–1.15cm³.mm/m².day.atm

PA6/66 Copolymer Grade Processing properties

Polymer injection moldingExcellent
Polymer extrusionAcceptable
Polymer thermoformingLimited use
Linear mold shrinkage0.8 – 2.6 %
Melt temperature232 – 304 °C
Mold temperature40 – 80 °C
Molding pressure range68.8 – 138 MPa

PA6/66 Copolymer Grade Durability

Water (fresh)Excellent
Water (salt)Acceptable
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisLimited use
Strong alkalisLimited use
Organic solventsAcceptable
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySlow-burning